Film grade hdpe 5000s high density polyethylene HDPE virgin recycled granules HDPE with low price CAS NO.9002-88-4
- FOB Price: USD: 850.00-1,000.00 /Metric Ton Get Latest Price
- Min.Order: 0 Metric Ton
- Payment Terms: T/T
- Product Details
Keywords
- 9002-88-4
- HDPE
- Polyethylene
Quick Details
- ProName: Film grade hdpe 5000s high density pol...
- CasNo: 9002-88-4
- Appearance: granular
- Application: Used for plastic products, as BAG,cup,...
- DeliveryTime: 45days after pay balance
- PackAge: 1kg/bag; 25kg/drum, or as customer's r...
- Port: Qingdao/Tianjin/Shanghai
- ProductionCapacity: 100 Metric Ton/Week
- Purity: 99.99
- Storage: Cool and dry place
- Transportation: by sea by air by express
- LimitNum: 0 Metric Ton
Superiority
Details
general application:
1.injection product: the turnover box, bottle caps, barrel class, hats, food containers, plate, dustbin, box etc
2.blow molding products: hollow molding products, such as various series blow molding barrel, containers, bottles of class, cosmetics,the petrol tank, daily product, etc
3.blow film product:foodstuff packing bag,groceries shopping bags, chemical fertilizer lined with film, etc
4.extruded product: pipe,tube mainly used in gas transportation, public water and chemicals transport, such as building materials, gas pipe, hot water drain pipe etc: sheet material is mainly used in the seat, suitcase, handling containers.etc
item | test condition | test method | value | unit |
density | iso 1183 | 0.944-0.955 | g/cm3 | |
mfr | 190°c/2.16kg | iso 1133 | 0.03-0.07 | g/10min |
tensile strength at yield | iso 527-2 | 22 | mpa | |
elongation at break | iso 527-2 | >350 | % | |
escr | f50,50°c,100% | astm d-1693a | 1000 | h |
vicat | astm d-1525 | 126 | °c |
blown grade
item | test condition | test method | value | unit |
density | iso 1183 | 0.950~0.955 | g/cm | |
mfr | 190°c/2.16kg | iso 1133 | 1.7~2.5 | g/10min |
tensile strength at yield | iso 527-2 | 24 | mpa | |
elongation at break | iso 527-2 | >600 | % |
injection grade
item | test condition | test method | value | unit |
mfr | 190°c/2.16kg | astm d-1238 | 20 | g/10min |
density | --- | astm d-792 | 0.954 | g/cm 3 |
tensile strength at yiled | --- | astm d-638 | 28 | mpa |
elongation at break | --- | astm d-638 | 250 | % |
impact tensile strength | --- | astm d-1822 | 42 | kj/m 2 |
escr | astm d-1693 | 3 | --- | |
vacit | --- | astm d-1525 | 127 | °c |